Issue 50
R. Boutelidja et alii, Frattura ed Integrità Strutturale, 50 (2019) 98-111; DOI: 10.3221/IGF-ESIS.50.10 109 Figure 15 : Probability to initiate a leak. Fig. 17 regroups the leak probability curves for the 4 cases studied. The effect of temperature depends on the triggering temperature of the Heat-up and Cool-down cycle. Figure 16 : Damage versus temperature. Figure 17 : Probability to have a leak.