L. Restuccia, Frattura ed Integrità Strutturale, 49 (2019) 676-689; DOI: 10.3221/IGF-ESIS.49.61 683 Figure 6 : S Results of XRD analysis for all the retained fraction of Recycled Washed Sand. Figure 7 : Particular of a grain of 0.16 mm of RSw. Figure 8 : Particular of a grain of 1.00 mm of RSw. C=calcite, Cl=clinochlore, Pa=paragonite, P=phlogopite, Q= quartz