H. S. Patil et alii, Frattura ed Integrità Strutturale, 48 (2019) 377-384; DOI: 10.3221/IGF-ESIS.48.36 382 observed. Based upon the cooling rate and stabilizing agent, the microstructures are grown at fusion zone. Structural morphology of C.P. titanium sheet is altered with respect to heat input consisting of α-phase bounded by β-phase and it is evident in Fig. 6. Figure 4: Microstructures structures of C.P titanium and various TIG welded samples. Figure 5: (a) optical micrographs of TIG weld profile of Titanium Gr-2, and (b-d) optical micrographs showing grain structures in the BM, HAZ and FZ Figure 6: Fusion Zone Microstructures for Titanium welds.