K.I. Tserpes et alii, Frattura ed Integrità Strutturale, 46 (2018) 73-83; DOI: 10.3221/IGF-ESIS.46.08 80 Figure 10 : Resistance to applied load mapping, at 300nm of displacement for a grid of 70 70 μ m 2 for MWCNT/PP 2 wt% specimen. Figure 11 : Elastic modulus mapping, at 300 nm of displacement for a grid of 70 70 μ m 2 for MWCNT/PP 2 wt% specimen. (a) (b) Figure 12 : (a) H / E and (b) H 3 / E 2 of MWCNT/PP 2 wt% specimen. Figure 13 : Contact pressure (as resistance to applied load) mapping, at 300nm of displacement for a grid of 70 μ m 2 for polypropylene with 2 % CNTs.